Low Carbon Ferromanganese
Specifications
| Material
Description: |
Low
Carbon Ferromanganese (L.C. FeMn) |
| Chemistry: |
| Mn |
80.0-95.0% |
| C |
0.75%
max. |
| Si |
1.2%
max. |
| P |
0.20%
max. |
| S |
0.10%
max. |
|
| Size: |
| 2" x
1/2" |
| Customized
sizing available upon request. |
|
| Bulk
Density: |
260
lb./cu. ft. |
| Apparent
Density: |
7.2
gm/cubic centimeter |
| Approximate
Melting Range: |
2310 °F
Liquidus
2100 °F Solidus |
| Application: |
In
cast iron, manganese is used mainly to counteract the bad
effects of sulfur. In steel, manganese acts as a deoxidizer
and combines with sulfur, thereby improving the hot-working
properties of the steel. Also improves the strength, toughness. |
| Country
of Origin: |
South
Africa, USA |
| Warehouse(s): |
Birmingham,
AL
Chicago, IL
East Liverpool, OH
Milwaukee, WI |
|
| Effective
Date: 8/20/13 |
 |
Please
Note:
Product specifications are subject to change
|
 |